Ordinary Portland Cement: Composition and Bogues Materials

Ordinary Portland Cement is a finely powdered grayish material made from a mixture of calcareous (such as limestone or chalk) and argillaceous materials and/or other silica, alumina, or iron oxide-bearing materials (e.g. clay and shale).

  • Named After: Portland, United Kingdom, due to its resemblance to stone quarried there.
  • Discovery: Discovered by Joseph Aspin of Yorkshire.
  • Manufacturing Process: Involves burning the mixture at a high temperature (1400-1450°C) and grinding the resulting clinker.

Manufacturing Process

  • Mixing: Two parts of calcareous material and one part of argillaceous material are mixed, crushed, and ground.
  • Burning: The finely ground powder is burned in a rotary kiln to white heat and fused into clinkers.
  • Grinding: The clinkers are cooled and ground to the required fineness.
  • Addition of Gypsum: Gypsum or air-entraining agent is added after the burning process.

Chemical Composition of Portland Cement

ConstituentsChemical FormulaPercentage (%)
LimeCaO60-67
SilicaSiO217-25
AluminaAl2O33-8
Iron-oxideFe2O30.5-6
MagnesiaMgO0.1-4
Sulphur trioxideSO31-3
Alkalies (Soda and Potash)Na2O+ K2O0.2-1.3

During the burning and fusion process of Portland cement, the constituent materials undergo chemical reactions to form various mineral compounds.

In August 1934, Professor P.H. Bogue and W. Lerch studied the hydration reactions of these mineral compounds with water and published their finding in the paper “Hydration of Portland Cement Compounds.” And from his name, these mineral compounds are also commonly referred to as Bogue compounds (sometimes called phases).

Mineral Compounds in Portland Cement (Bogues Compounds)

Mineral CompoundsConventional FormulaPercentage (%)
Tri-calcium silicate (Alite, C3S)3CaO.SiO250-70%
Di-calcium silicate (Belite, C2S)2CaO.SiO215-30%
Tri-calcium aluminate (Celite, C3A)3CaO.Al2O35-10%
Tetra-calcium alumino-ferrite (Felite, C4AF)4CaO.Al2O3.Fe2O35-15%

When cement is mixed with water, it forms a cement paste. This paste undergoes a process of setting and hardening.

  • Setting: The cement paste transitions from a plastic state to a stiff solid state. It gains minimal compressive strength during this phase.
  • Hardening: The compressive strength of the cement paste increases over time as hydration continues.

Role of Tricalcium Aluminate (C3A) in Cement

  • Initial Setting and Early Hardening: C3A is responsible for the rapid initial setting and early hardening of concrete.
  • Retardant: Gypsum (CaSO4) is added to control the rapid setting of C3A.
  • Strength Development: C3A contributes to early strength but its maximum strengthening effect is within 24 hours.

Role of C3S, C2S and C4AF

  • C3S and C2S: These compounds make up a significant portion of cement (70-75%). C3S provides both early and ultimate strength, while C2S contributes to strength after seven days and provides long-term durability.
  • C3A and C4AF: C3A combines with C4AF to form hydrated products that contribute moderate strength to concrete.

Read More: Adulteration of Cement: Test, Chemical & Instrumental Analysis

Reference:

Leave a Comment